Xuba i-10% ye-3235 kunye ne-polyester TPU ngokulinganayo, uze uphoswe ngokuthe ngqo ukufumana ifilimu enobunzima be-microns ezili-10. Vavanya inkungu, ukuhanjiswa kokukhanya, kunye neglosi, kwaye, thelekisa nemveliso ye-TPU ekhuphisanayo.
IBanga | 3235 | |
Imbonakalo | I-White Matt Pellet | |
Isiseko se-resin | TPU | |
Ukuqina | Unxweme A | 70 |
Isalathisi sokunyibilika ( 190℃, 2. 16KG ) | g/10min | 5-15 ( ixabiso eliqhelekileyo ) |
Ukuguquguquka | (%) | ≤2 |
Amanqanaba okongeza phakathi kwe-5.0 ~ 10% ayacetyiswa. Ingasetyenziswa kwinkqubo yokudibanisa ye-classical melt efana ne-Single / Twin screw extruders, ukubumba inaliti. Umxube womzimba kunye neepellets zepolymer ezinyulu ziyacetyiswa.
I-25 kg / ibhegi, ingxowa yeplastiki engenamanzi ene-PE yangaphakathi yebhegi.
Uthutho njengekhemikhali engeyongozi. Gcina kwindawo epholileyo, nengena umoya.
Iimpawu zokuqala zihlala zingaguquki kwiinyanga ezingama-24 ukusuka kumhla wemveliso, ukuba zigcinwe kwindawo ecetyiswayo.